The density of seasoned & dry wood are indicated in the table below:

Solid

Density

(103 kg/m3) 

(lb/ft3) 

Alder

0.4 - 0.7

26 - 42

Afrormosia

0.71

Agba

0.51

Apple

0.65 - 0.85

41 - 52

Ash, white

0.65 - 0.85

40 - 53

Ash, black

0.54

33

Ash, European

0.71

Aspen

0.42

26

Balsa

0.16

7 - 9

Bamboo

0.3 - 0.4

19 - 25

Basswood

0.3 - 0.6

20 - 37

Beech

0.7 - 0.9

32 - 56

Birch, British

0.67

42

Birch, European

0.67

Box

0.95 - 1.2

59 - 72

Butternut

0.38

24

Cedar of Lebanon

0.58

Cedar, western red

0.38

23

Cherry, European

0.63

43- 56

Chestnut, sweet

0.56

30

Cottonwood

0.41

25

Cypress

0.51

32

Dogwood

0.75

47

Douglas Fir

0.53

33

Ebony

1.1 - 1.3

69 - 83

Elm, American

0.57

35

Elm, English

0.55 - 0.6

34 - 37

Elm, Dutch

0.56

Elm, Wych

0.69

Elm, Rock

0.82

50

Gaboon

0.43

Greenheart

1.04

Gum, Black

0.59

36

Gum, Blue

0.82

50

Gum, Red

0.54

35

Hackberry

0.62

38

Hemlock, western

0.50

Hickory

0.83

37 - 58

Holly

0.75

47

Iroko

0.66

Juniper

0.55

35

Keruing

0.74

Larch

0.5 - 0.55

31 - 35

Lignum Vitae

1.17 - 1.33

73 - 83

Lime, European

0.56

Locust

0.65 - 0.7

42 - 44

Logwood

0.9

57

Madrone

0.74

45

Magnolia

0.57

35

Mahogany, African

0.5 - 0.85

31 - 53

Mahogany, Cuban

0.66

40

Mahogany, Honduras

0.65

41

Mahogany, Spanish

0.85

53

Maple

0.6 - 0.75

39 - 47

Meranti, dark red

0.71

Myrtle

0.66

40

Oak

0.6 - 0.9

37 - 56

Oak, American Red

0.74

45

Oak, American White

0.77

47

Oak, English Brown

0.74

45

Obeche

0.39

Oregon Pine

0.53

33

Parana Pine

0.56

35

Pear

0.6 - 0.7

38 - 45

Pecan

0.77

47

Persimmon

0.9

55

Philippine Red Luan

0.59

36

Pine, pitch

0.67

52 - 53

Pine, Corsican

0.51

Pine, radiata

0.48

Pine, Scots

0.51

Pine, white

0.35 - 0.5

22 - 31

Pine, yellow

0.42

23 - 37

Plane, European

0.64

Plum

0.65 - 0.8

41 - 49

Poplar

0.35 - 0.5

22 - 31

Ramin

0.67

Redwood, American

0.45

28

Redwood, European

0.51

32

Rosewood, Bolivian

0.82

50

Rosewood, East Indian

0.90

55

Sapele

0.64

Satinwood

0.95

59

Spruce

0.4 - 0.7

25 - 44

Spruce, Canadian

0.45

28

Spruce, Norway

0.43

Spruce, Sitka

0.45

28

Spruce, western white

0.45

Sycamore

0.4 - 0.6

24 - 37

Tanguile

0.64

39

Teak, Indian

0.65 - 0.9

41 - 55

Teak, African

0.98

61

Teak, Burma

0.74

45

Utile

0.66

Walnut

0.65 - 0.7

40 - 43

Walnut, Amer Black

0.63

38

Walnut, Claro

0.49

30

Walnut, European

0.57

35

Water gum

1

62

Whitewood, European

0.47

Willow

0.4 - 0.6

24 - 37

Yew

0.67

Zebrawood

0.79

48

(Note: 1 kg/m3 = 0.001 g/cm3 = 0.0005780 oz/in3 = 0.16036 oz/gal (Imperial) = 0.1335 oz/gal (U.S.) = 0.0624 lb/ft3 = 0.000036127 lb/in3 = 1.6856 lb/yd3 = 0.010022 lb/gal (Imperial) = 0.008345 lb/gal (U.S) = 0.0007525 ton/yd3 .)

After felling, timber will lose moisture to align itself with the atmospheric conditions. Moisture content should be lower than 20% to stop fungal attack. Seasoning is the name of the process where moisture content is reduced to the appropriate level for proposed use. Shrinkage will occur as a result of the moisture loss - typical 3-4% across the grain.

Sunco Machinery Wood Shavings Dryer can be used to drying all kinds of wood shavings. After being dried by our wood shavings dryer, the moisture content of wood shavings can be below 15%.

Inquiry
Note: Please feel free to give your inquiry in the form below. We will reply you with details within 24 hours.
Topic: *
Company:
Name: *
Tel: *
E-mail: *
Message: